Abstract

We present differential-scanning-calorimetry curves and infrared spectra taken during the temperature cycling of stoichiometrically pure RbC60 powder. In addition to the three known phases (high-temperature fcc, ortho-I, and ortho-II), we see evidence for an intermediate structure around 300 K, observed previously by ESR and x-ray diffraction. This phase is obtained both by quenching from high temperature and by warming up the ortho-II structure. Its infrared spectrum is identical to that of the high-temperature fcc phase, indicating a structure containing C60- monomers.

Original languageEnglish
Pages (from-to)11488-11491
Number of pages4
JournalPhysical Review B
Volume52
Issue number15
DOIs
Publication statusPublished - 1995

Fingerprint

Differential scanning calorimetry
heat measurement
Infrared radiation
scanning
room temperature
infrared spectra
Temperature
x ray diffraction
monomers
quenching
Powders
Paramagnetic resonance
Quenching
cycles
heating
Diffraction
Monomers
curves
X rays
temperature

ASJC Scopus subject areas

  • Condensed Matter Physics

Cite this

Infrared and differential-scanning-calorimetry study of the room-temperature cubic phase of RbC60. / Kamarás, K.; Gránásy, L.; Tanner, D. B.; Forró, L.

In: Physical Review B, Vol. 52, No. 15, 1995, p. 11488-11491.

Research output: Article

Kamarás, K. ; Gránásy, L. ; Tanner, D. B. ; Forró, L. / Infrared and differential-scanning-calorimetry study of the room-temperature cubic phase of RbC60. In: Physical Review B. 1995 ; Vol. 52, No. 15. pp. 11488-11491.
@article{86ea8e6192ad45d38c4534ce87125242,
title = "Infrared and differential-scanning-calorimetry study of the room-temperature cubic phase of RbC60",
abstract = "We present differential-scanning-calorimetry curves and infrared spectra taken during the temperature cycling of stoichiometrically pure RbC60 powder. In addition to the three known phases (high-temperature fcc, ortho-I, and ortho-II), we see evidence for an intermediate structure around 300 K, observed previously by ESR and x-ray diffraction. This phase is obtained both by quenching from high temperature and by warming up the ortho-II structure. Its infrared spectrum is identical to that of the high-temperature fcc phase, indicating a structure containing C60- monomers.",
author = "K. Kamar{\'a}s and L. Gr{\'a}n{\'a}sy and Tanner, {D. B.} and L. Forr{\'o}",
year = "1995",
doi = "10.1103/PhysRevB.52.11488",
language = "English",
volume = "52",
pages = "11488--11491",
journal = "Physical Review B-Condensed Matter",
issn = "0163-1829",
publisher = "American Physical Society",
number = "15",

}

TY - JOUR

T1 - Infrared and differential-scanning-calorimetry study of the room-temperature cubic phase of RbC60

AU - Kamarás, K.

AU - Gránásy, L.

AU - Tanner, D. B.

AU - Forró, L.

PY - 1995

Y1 - 1995

N2 - We present differential-scanning-calorimetry curves and infrared spectra taken during the temperature cycling of stoichiometrically pure RbC60 powder. In addition to the three known phases (high-temperature fcc, ortho-I, and ortho-II), we see evidence for an intermediate structure around 300 K, observed previously by ESR and x-ray diffraction. This phase is obtained both by quenching from high temperature and by warming up the ortho-II structure. Its infrared spectrum is identical to that of the high-temperature fcc phase, indicating a structure containing C60- monomers.

AB - We present differential-scanning-calorimetry curves and infrared spectra taken during the temperature cycling of stoichiometrically pure RbC60 powder. In addition to the three known phases (high-temperature fcc, ortho-I, and ortho-II), we see evidence for an intermediate structure around 300 K, observed previously by ESR and x-ray diffraction. This phase is obtained both by quenching from high temperature and by warming up the ortho-II structure. Its infrared spectrum is identical to that of the high-temperature fcc phase, indicating a structure containing C60- monomers.

UR - http://www.scopus.com/inward/record.url?scp=0003650227&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0003650227&partnerID=8YFLogxK

U2 - 10.1103/PhysRevB.52.11488

DO - 10.1103/PhysRevB.52.11488

M3 - Article

AN - SCOPUS:0003650227

VL - 52

SP - 11488

EP - 11491

JO - Physical Review B-Condensed Matter

JF - Physical Review B-Condensed Matter

SN - 0163-1829

IS - 15

ER -