Original language | English |
---|---|
Pages (from-to) | 943-946 |
Number of pages | 4 |
Journal | Scripta Metallurgica |
Volume | 19 |
Issue number | 8 |
DOIs | |
Publication status | Published - 1985 |
Fingerprint
ASJC Scopus subject areas
- Engineering(all)
Cite this
A differential scanning calorimetry study of the release of stored energy in an AlFe alloy. / Lendvai, J.; Honyek, G.; Juhász, A.; Kovács, I.
In: Scripta Metallurgica, Vol. 19, No. 8, 1985, p. 943-946.Research output: Article
}
TY - JOUR
T1 - A differential scanning calorimetry study of the release of stored energy in an AlFe alloy
AU - Lendvai, J.
AU - Honyek, G.
AU - Juhász, A.
AU - Kovács, I.
PY - 1985
Y1 - 1985
UR - http://www.scopus.com/inward/record.url?scp=0022108102&partnerID=8YFLogxK
UR - http://www.scopus.com/inward/citedby.url?scp=0022108102&partnerID=8YFLogxK
U2 - 10.1016/0036-9748(85)90288-1
DO - 10.1016/0036-9748(85)90288-1
M3 - Article
AN - SCOPUS:0022108102
VL - 19
SP - 943
EP - 946
JO - Scripta Materialia
JF - Scripta Materialia
SN - 1359-6462
IS - 8
ER -