Abstract

The present study aims at the quantitative decomposition of various photoelectron peaks observed in spectra of Pt-black surfaces as a function of Ar** plus ion bombardment charge density.

Original languageEnglish
Title of host publicationSurface and Interface Analysis
Pages251-252
Number of pages2
Volume9
Edition1-6
Publication statusPublished - Jul 1986
EventSurf and Interface Anal, ECASIA 85, Proc of the Eur Conf on Appl of Surf and Interface Anal - Veldhoven, Neth
Duration: Oct 14 1986Oct 18 1986

Other

OtherSurf and Interface Anal, ECASIA 85, Proc of the Eur Conf on Appl of Surf and Interface Anal
CityVeldhoven, Neth
Period10/14/8610/18/86

Fingerprint

Ion bombardment
Photoelectrons
Charge density
bombardment
photoelectrons
X ray photoelectron spectroscopy
Decomposition
decomposition
ions

ASJC Scopus subject areas

  • Colloid and Surface Chemistry
  • Physical and Theoretical Chemistry

Cite this

Kövér, L., Toth, J., & Paál, Z. (1986). SURFACE ANALYSIS OF Pt-BLACK BY XPS. In Surface and Interface Analysis (1-6 ed., Vol. 9, pp. 251-252)

SURFACE ANALYSIS OF Pt-BLACK BY XPS. / Kövér, L.; Toth, J.; Paál, Z.

Surface and Interface Analysis. Vol. 9 1-6. ed. 1986. p. 251-252.

Research output: Chapter in Book/Report/Conference proceedingChapter

Kövér, L, Toth, J & Paál, Z 1986, SURFACE ANALYSIS OF Pt-BLACK BY XPS. in Surface and Interface Analysis. 1-6 edn, vol. 9, pp. 251-252, Surf and Interface Anal, ECASIA 85, Proc of the Eur Conf on Appl of Surf and Interface Anal, Veldhoven, Neth, 10/14/86.
Kövér L, Toth J, Paál Z. SURFACE ANALYSIS OF Pt-BLACK BY XPS. In Surface and Interface Analysis. 1-6 ed. Vol. 9. 1986. p. 251-252
Kövér, L. ; Toth, J. ; Paál, Z. / SURFACE ANALYSIS OF Pt-BLACK BY XPS. Surface and Interface Analysis. Vol. 9 1-6. ed. 1986. pp. 251-252
@inbook{97df1db602cc4852bbb5d52a234a379b,
title = "SURFACE ANALYSIS OF Pt-BLACK BY XPS.",
abstract = "The present study aims at the quantitative decomposition of various photoelectron peaks observed in spectra of Pt-black surfaces as a function of Ar** plus ion bombardment charge density.",
author = "L. K{\"o}v{\'e}r and J. Toth and Z. Pa{\'a}l",
year = "1986",
month = "7",
language = "English",
isbn = "0471916607",
volume = "9",
pages = "251--252",
booktitle = "Surface and Interface Analysis",
edition = "1-6",

}

TY - CHAP

T1 - SURFACE ANALYSIS OF Pt-BLACK BY XPS.

AU - Kövér, L.

AU - Toth, J.

AU - Paál, Z.

PY - 1986/7

Y1 - 1986/7

N2 - The present study aims at the quantitative decomposition of various photoelectron peaks observed in spectra of Pt-black surfaces as a function of Ar** plus ion bombardment charge density.

AB - The present study aims at the quantitative decomposition of various photoelectron peaks observed in spectra of Pt-black surfaces as a function of Ar** plus ion bombardment charge density.

UR - http://www.scopus.com/inward/record.url?scp=0022743174&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0022743174&partnerID=8YFLogxK

M3 - Chapter

AN - SCOPUS:0022743174

SN - 0471916607

VL - 9

SP - 251

EP - 252

BT - Surface and Interface Analysis

ER -