Abstract

Hydrophilic graphite oxide (GO) of lamellar structure was prepared by oxidation of graphite; the thickness of the individual lamellae was 6.1 Å. GO was hydrophobized by n-alkylammonium cations, and the GO-organocomplex nanocomposites were swollen in organic solvents of various polarities (ethanol, toluene, cyclohexane, n-heptane) and their binary mixtures. The binary liquid composition determined the size (15-45 Å) of the lamellar GO nanostructures. Interlamellar swelling was quantitatively characterized by XRD experiments, determination of liquid sorption excess isotherms and flow microcalorimetry.

Original languageEnglish
Pages (from-to)570-576
Number of pages7
JournalColloid & Polymer Science
Volume276
Issue number7
DOIs
Publication statusPublished - Jul 1998

Fingerprint

Graphite
sorption
Oxides
Sorption
Nanostructures
graphite
oxides
Liquids
liquids
Lamellar structures
Toluene
Heptane
lamella
Cyclohexane
heptanes
Binary mixtures
swelling
cyclohexane
Organic solvents
binary mixtures

Keywords

  • Graphite oxides
  • Liquid adsorption
  • Microcalorimetry
  • Nanostructures
  • Swelling

ASJC Scopus subject areas

  • Physical and Theoretical Chemistry
  • Polymers and Plastics
  • Materials Chemistry
  • Colloid and Surface Chemistry

Cite this

Selective liquid sorption properties of hydrophobized graphite oxide nanostructures. / Dékány, I.; Krüger-Grasser, R.; Weiss, A.

In: Colloid & Polymer Science, Vol. 276, No. 7, 07.1998, p. 570-576.

Research output: Contribution to journalArticle

Dékány, I. ; Krüger-Grasser, R. ; Weiss, A. / Selective liquid sorption properties of hydrophobized graphite oxide nanostructures. In: Colloid & Polymer Science. 1998 ; Vol. 276, No. 7. pp. 570-576.
@article{e6dabb94de15494eb63c25fb9a4ab2c3,
title = "Selective liquid sorption properties of hydrophobized graphite oxide nanostructures",
abstract = "Hydrophilic graphite oxide (GO) of lamellar structure was prepared by oxidation of graphite; the thickness of the individual lamellae was 6.1 {\AA}. GO was hydrophobized by n-alkylammonium cations, and the GO-organocomplex nanocomposites were swollen in organic solvents of various polarities (ethanol, toluene, cyclohexane, n-heptane) and their binary mixtures. The binary liquid composition determined the size (15-45 {\AA}) of the lamellar GO nanostructures. Interlamellar swelling was quantitatively characterized by XRD experiments, determination of liquid sorption excess isotherms and flow microcalorimetry.",
keywords = "Graphite oxides, Liquid adsorption, Microcalorimetry, Nanostructures, Swelling",
author = "I. D{\'e}k{\'a}ny and R. Kr{\"u}ger-Grasser and A. Weiss",
year = "1998",
month = "7",
doi = "10.1007/s003960050283",
language = "English",
volume = "276",
pages = "570--576",
journal = "Kolloid Zeitschrift",
issn = "0303-402X",
publisher = "Springer Verlag",
number = "7",

}

TY - JOUR

T1 - Selective liquid sorption properties of hydrophobized graphite oxide nanostructures

AU - Dékány, I.

AU - Krüger-Grasser, R.

AU - Weiss, A.

PY - 1998/7

Y1 - 1998/7

N2 - Hydrophilic graphite oxide (GO) of lamellar structure was prepared by oxidation of graphite; the thickness of the individual lamellae was 6.1 Å. GO was hydrophobized by n-alkylammonium cations, and the GO-organocomplex nanocomposites were swollen in organic solvents of various polarities (ethanol, toluene, cyclohexane, n-heptane) and their binary mixtures. The binary liquid composition determined the size (15-45 Å) of the lamellar GO nanostructures. Interlamellar swelling was quantitatively characterized by XRD experiments, determination of liquid sorption excess isotherms and flow microcalorimetry.

AB - Hydrophilic graphite oxide (GO) of lamellar structure was prepared by oxidation of graphite; the thickness of the individual lamellae was 6.1 Å. GO was hydrophobized by n-alkylammonium cations, and the GO-organocomplex nanocomposites were swollen in organic solvents of various polarities (ethanol, toluene, cyclohexane, n-heptane) and their binary mixtures. The binary liquid composition determined the size (15-45 Å) of the lamellar GO nanostructures. Interlamellar swelling was quantitatively characterized by XRD experiments, determination of liquid sorption excess isotherms and flow microcalorimetry.

KW - Graphite oxides

KW - Liquid adsorption

KW - Microcalorimetry

KW - Nanostructures

KW - Swelling

UR - http://www.scopus.com/inward/record.url?scp=0038121492&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0038121492&partnerID=8YFLogxK

U2 - 10.1007/s003960050283

DO - 10.1007/s003960050283

M3 - Article

AN - SCOPUS:0038121492

VL - 276

SP - 570

EP - 576

JO - Kolloid Zeitschrift

JF - Kolloid Zeitschrift

SN - 0303-402X

IS - 7

ER -