Quantitative estimation of the reinforcing effect of layered silicates in PP nanocomposites

L. Százdi, Béla Pukánszky, G. Julius Vancso, B. Pukánszky

Research output: Contribution to journalArticle

76 Citations (Scopus)

Abstract

Various polypropylene/layered silicate composites were prepared with different silicate contents. Montmorillonites with and without organophilization as well as three maleinated polypropylenes were used to change the extent of exfoliation and hence the properties of the composites. Structure was characterized by X-ray diffraction (XRD), scanning (SEM) as well as transmission electron microscopy (TEM) and tensile properties were also measured. The analysis of the tensile yield stress values of a large number of composites showed a broad range of variation in mechanical properties. XRD and TEM results do not reflect the differences in properties and they usually do not give quantitative information about the extent of exfoliation either. PP/clay composites containing maleinated PP, which do not exhibit a silicate reflection in XRD, may have very poor mechanical properties indicating small extent of exfoliation. The composition dependence of tensile yield stress of these composites may be described and evaluated quantitatively by a simple model developed earlier for particulate filled polymers. The use of a few simple assumptions most of which are supported by previous results allows us to estimate the extent of exfoliation quantitatively. The tensile yield stress of about 40 composites was analyzed with the model. Some of the composites were prepared by us, while results on others were taken from papers published in the literature. The analysis indicated that the extent of exfoliation is very low in most composites; it reaches maximum 8% of the theoretically possible value in the best case. This result is in agreement with our observation that complete exfoliation can be seldom reached in thermoplastic/clay composites; the structure is complex and hierarchical including large particles and individual silicate layers. The results prove that further efforts must be done to increase the extent of exfoliation in order to achieve reinforcement levels forecasted earlier.

Original languageEnglish
Pages (from-to)4638-4648
Number of pages11
JournalPolymer (United Kingdom)
Volume47
Issue number13
DOIs
Publication statusPublished - Jun 14 2006

Fingerprint

Silicates
Nanocomposites
Composite materials
Yield stress
Polypropylenes
X ray diffraction
Clay
Transmission electron microscopy
Filled polymers
Mechanical properties
Tensile properties
Thermoplastics
Reinforcement
Scanning
Scanning electron microscopy

Keywords

  • Layered silicates
  • Nanocomposites
  • Polypropylene

ASJC Scopus subject areas

  • Organic Chemistry
  • Polymers and Plastics

Cite this

Quantitative estimation of the reinforcing effect of layered silicates in PP nanocomposites. / Százdi, L.; Pukánszky, Béla; Vancso, G. Julius; Pukánszky, B.

In: Polymer (United Kingdom), Vol. 47, No. 13, 14.06.2006, p. 4638-4648.

Research output: Contribution to journalArticle

@article{10c7a3228bea44269c69b1de72b8621c,
title = "Quantitative estimation of the reinforcing effect of layered silicates in PP nanocomposites",
abstract = "Various polypropylene/layered silicate composites were prepared with different silicate contents. Montmorillonites with and without organophilization as well as three maleinated polypropylenes were used to change the extent of exfoliation and hence the properties of the composites. Structure was characterized by X-ray diffraction (XRD), scanning (SEM) as well as transmission electron microscopy (TEM) and tensile properties were also measured. The analysis of the tensile yield stress values of a large number of composites showed a broad range of variation in mechanical properties. XRD and TEM results do not reflect the differences in properties and they usually do not give quantitative information about the extent of exfoliation either. PP/clay composites containing maleinated PP, which do not exhibit a silicate reflection in XRD, may have very poor mechanical properties indicating small extent of exfoliation. The composition dependence of tensile yield stress of these composites may be described and evaluated quantitatively by a simple model developed earlier for particulate filled polymers. The use of a few simple assumptions most of which are supported by previous results allows us to estimate the extent of exfoliation quantitatively. The tensile yield stress of about 40 composites was analyzed with the model. Some of the composites were prepared by us, while results on others were taken from papers published in the literature. The analysis indicated that the extent of exfoliation is very low in most composites; it reaches maximum 8{\%} of the theoretically possible value in the best case. This result is in agreement with our observation that complete exfoliation can be seldom reached in thermoplastic/clay composites; the structure is complex and hierarchical including large particles and individual silicate layers. The results prove that further efforts must be done to increase the extent of exfoliation in order to achieve reinforcement levels forecasted earlier.",
keywords = "Layered silicates, Nanocomposites, Polypropylene",
author = "L. Sz{\'a}zdi and B{\'e}la Puk{\'a}nszky and Vancso, {G. Julius} and B. Puk{\'a}nszky",
year = "2006",
month = "6",
day = "14",
doi = "10.1016/j.polymer.2006.04.053",
language = "English",
volume = "47",
pages = "4638--4648",
journal = "Polymer",
issn = "0032-3861",
publisher = "Elsevier BV",
number = "13",

}

TY - JOUR

T1 - Quantitative estimation of the reinforcing effect of layered silicates in PP nanocomposites

AU - Százdi, L.

AU - Pukánszky, Béla

AU - Vancso, G. Julius

AU - Pukánszky, B.

PY - 2006/6/14

Y1 - 2006/6/14

N2 - Various polypropylene/layered silicate composites were prepared with different silicate contents. Montmorillonites with and without organophilization as well as three maleinated polypropylenes were used to change the extent of exfoliation and hence the properties of the composites. Structure was characterized by X-ray diffraction (XRD), scanning (SEM) as well as transmission electron microscopy (TEM) and tensile properties were also measured. The analysis of the tensile yield stress values of a large number of composites showed a broad range of variation in mechanical properties. XRD and TEM results do not reflect the differences in properties and they usually do not give quantitative information about the extent of exfoliation either. PP/clay composites containing maleinated PP, which do not exhibit a silicate reflection in XRD, may have very poor mechanical properties indicating small extent of exfoliation. The composition dependence of tensile yield stress of these composites may be described and evaluated quantitatively by a simple model developed earlier for particulate filled polymers. The use of a few simple assumptions most of which are supported by previous results allows us to estimate the extent of exfoliation quantitatively. The tensile yield stress of about 40 composites was analyzed with the model. Some of the composites were prepared by us, while results on others were taken from papers published in the literature. The analysis indicated that the extent of exfoliation is very low in most composites; it reaches maximum 8% of the theoretically possible value in the best case. This result is in agreement with our observation that complete exfoliation can be seldom reached in thermoplastic/clay composites; the structure is complex and hierarchical including large particles and individual silicate layers. The results prove that further efforts must be done to increase the extent of exfoliation in order to achieve reinforcement levels forecasted earlier.

AB - Various polypropylene/layered silicate composites were prepared with different silicate contents. Montmorillonites with and without organophilization as well as three maleinated polypropylenes were used to change the extent of exfoliation and hence the properties of the composites. Structure was characterized by X-ray diffraction (XRD), scanning (SEM) as well as transmission electron microscopy (TEM) and tensile properties were also measured. The analysis of the tensile yield stress values of a large number of composites showed a broad range of variation in mechanical properties. XRD and TEM results do not reflect the differences in properties and they usually do not give quantitative information about the extent of exfoliation either. PP/clay composites containing maleinated PP, which do not exhibit a silicate reflection in XRD, may have very poor mechanical properties indicating small extent of exfoliation. The composition dependence of tensile yield stress of these composites may be described and evaluated quantitatively by a simple model developed earlier for particulate filled polymers. The use of a few simple assumptions most of which are supported by previous results allows us to estimate the extent of exfoliation quantitatively. The tensile yield stress of about 40 composites was analyzed with the model. Some of the composites were prepared by us, while results on others were taken from papers published in the literature. The analysis indicated that the extent of exfoliation is very low in most composites; it reaches maximum 8% of the theoretically possible value in the best case. This result is in agreement with our observation that complete exfoliation can be seldom reached in thermoplastic/clay composites; the structure is complex and hierarchical including large particles and individual silicate layers. The results prove that further efforts must be done to increase the extent of exfoliation in order to achieve reinforcement levels forecasted earlier.

KW - Layered silicates

KW - Nanocomposites

KW - Polypropylene

UR - http://www.scopus.com/inward/record.url?scp=33744911366&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=33744911366&partnerID=8YFLogxK

U2 - 10.1016/j.polymer.2006.04.053

DO - 10.1016/j.polymer.2006.04.053

M3 - Article

AN - SCOPUS:33744911366

VL - 47

SP - 4638

EP - 4648

JO - Polymer

JF - Polymer

SN - 0032-3861

IS - 13

ER -