Abstract

The quality of the drilled YBCO bulks and rings and the precision of the fitting of the YBCO rings joined together can be deduced with the elaborated method. In the case ofconcerted magnetization of tightly fitted rings and bulk the measured maximum flux density is approximately the same as it was prior to machining unless the material got damaged during machining. It is also a convenient method to test the material before the application of bulks and rings.

Original languageEnglish
Article number5067132
Pages (from-to)2183-2185
Number of pages3
JournalIEEE Transactions on Applied Superconductivity
Volume19
Issue number3
DOIs
Publication statusPublished - Jun 2009

Fingerprint

qualifications
machining
Machining
examination
Fluxes
rings
Magnetization
flux density
magnetization

Keywords

  • Machining
  • Magnetization processes
  • Superconductors

ASJC Scopus subject areas

  • Electrical and Electronic Engineering
  • Condensed Matter Physics
  • Electronic, Optical and Magnetic Materials

Cite this

Qualification of the machining and fitting precision of YBCO bulks and rings joined together via the examination of the trapped flux. / Kosa, J.; Vajda, I.; Farkas, L.

In: IEEE Transactions on Applied Superconductivity, Vol. 19, No. 3, 5067132, 06.2009, p. 2183-2185.

Research output: Contribution to journalArticle

@article{fc3b8bd73ed64339b2f285e188fd3b5c,
title = "Qualification of the machining and fitting precision of YBCO bulks and rings joined together via the examination of the trapped flux",
abstract = "The quality of the drilled YBCO bulks and rings and the precision of the fitting of the YBCO rings joined together can be deduced with the elaborated method. In the case ofconcerted magnetization of tightly fitted rings and bulk the measured maximum flux density is approximately the same as it was prior to machining unless the material got damaged during machining. It is also a convenient method to test the material before the application of bulks and rings.",
keywords = "Machining, Magnetization processes, Superconductors",
author = "J. Kosa and I. Vajda and L. Farkas",
year = "2009",
month = "6",
doi = "10.1109/TASC.2009.2017760",
language = "English",
volume = "19",
pages = "2183--2185",
journal = "IEEE Transactions on Applied Superconductivity",
issn = "1051-8223",
publisher = "Institute of Electrical and Electronics Engineers Inc.",
number = "3",

}

TY - JOUR

T1 - Qualification of the machining and fitting precision of YBCO bulks and rings joined together via the examination of the trapped flux

AU - Kosa, J.

AU - Vajda, I.

AU - Farkas, L.

PY - 2009/6

Y1 - 2009/6

N2 - The quality of the drilled YBCO bulks and rings and the precision of the fitting of the YBCO rings joined together can be deduced with the elaborated method. In the case ofconcerted magnetization of tightly fitted rings and bulk the measured maximum flux density is approximately the same as it was prior to machining unless the material got damaged during machining. It is also a convenient method to test the material before the application of bulks and rings.

AB - The quality of the drilled YBCO bulks and rings and the precision of the fitting of the YBCO rings joined together can be deduced with the elaborated method. In the case ofconcerted magnetization of tightly fitted rings and bulk the measured maximum flux density is approximately the same as it was prior to machining unless the material got damaged during machining. It is also a convenient method to test the material before the application of bulks and rings.

KW - Machining

KW - Magnetization processes

KW - Superconductors

UR - http://www.scopus.com/inward/record.url?scp=68649092207&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=68649092207&partnerID=8YFLogxK

U2 - 10.1109/TASC.2009.2017760

DO - 10.1109/TASC.2009.2017760

M3 - Article

AN - SCOPUS:68649092207

VL - 19

SP - 2183

EP - 2185

JO - IEEE Transactions on Applied Superconductivity

JF - IEEE Transactions on Applied Superconductivity

SN - 1051-8223

IS - 3

M1 - 5067132

ER -