Abstract

In this investigation we observed the interface between Wiron 99 (Bego) dental Ni-Cr alloy and Vision (Wohlwend AG) ceramic opaquer with SEM. In the system there are intermediate phases coming from a solid phase rection which play an essential role in the metal-ceramic bond. The analytical methods showed that in this phases the content of Ni and Cr charge not monotonously from alloy to ceramic which shows strong chemical effects (the selective affinity of Cr and Ni). The concentration of Cr after the alloy surface increases in a 1-1.5 microns layer, where its concentration is higher than at the alloy, while the concentration of Ni decrease in this layer. Than at the ceramic side of the reaction zone the concentration of Ni increases in a 1-1.5 microns wide layer where its concentration is near upon that one in the alloy.

Original languageHungarian
Pages (from-to)121-127
Number of pages7
JournalFogorvosi szemle
Volume92
Issue number4
Publication statusPublished - 1999

Fingerprint

Ceramics
Electron Scanning Microscopy
Tooth
Metals

Cite this

Ni-Cr ötvözet és kerámia határfelület pásztázó elektronmikroszkópos (PEM) vizsgálata. / Hegedüs, C.; Kökényesi, V.; Imre, A.; Beke, D.

In: Fogorvosi szemle, Vol. 92, No. 4, 1999, p. 121-127.

Research output: Contribution to journalArticle

Hegedüs, C. ; Kökényesi, V. ; Imre, A. ; Beke, D. / Ni-Cr ötvözet és kerámia határfelület pásztázó elektronmikroszkópos (PEM) vizsgálata. In: Fogorvosi szemle. 1999 ; Vol. 92, No. 4. pp. 121-127.
@article{4cd8438ea3bf4b8b9e9a9a4d76b77d69,
title = "Ni-Cr {\"o}tv{\"o}zet {\'e}s ker{\'a}mia hat{\'a}rfel{\"u}let p{\'a}szt{\'a}z{\'o} elektronmikroszk{\'o}pos (PEM) vizsg{\'a}lata.",
abstract = "In this investigation we observed the interface between Wiron 99 (Bego) dental Ni-Cr alloy and Vision (Wohlwend AG) ceramic opaquer with SEM. In the system there are intermediate phases coming from a solid phase rection which play an essential role in the metal-ceramic bond. The analytical methods showed that in this phases the content of Ni and Cr charge not monotonously from alloy to ceramic which shows strong chemical effects (the selective affinity of Cr and Ni). The concentration of Cr after the alloy surface increases in a 1-1.5 microns layer, where its concentration is higher than at the alloy, while the concentration of Ni decrease in this layer. Than at the ceramic side of the reaction zone the concentration of Ni increases in a 1-1.5 microns wide layer where its concentration is near upon that one in the alloy.",
author = "C. Heged{\"u}s and V. K{\"o}k{\'e}nyesi and A. Imre and D. Beke",
year = "1999",
language = "Hungarian",
volume = "92",
pages = "121--127",
journal = "Fogorvosi szemle",
issn = "0015-5314",
publisher = "Ifjusagi Lapkiado Vallalat",
number = "4",

}

TY - JOUR

T1 - Ni-Cr ötvözet és kerámia határfelület pásztázó elektronmikroszkópos (PEM) vizsgálata.

AU - Hegedüs, C.

AU - Kökényesi, V.

AU - Imre, A.

AU - Beke, D.

PY - 1999

Y1 - 1999

N2 - In this investigation we observed the interface between Wiron 99 (Bego) dental Ni-Cr alloy and Vision (Wohlwend AG) ceramic opaquer with SEM. In the system there are intermediate phases coming from a solid phase rection which play an essential role in the metal-ceramic bond. The analytical methods showed that in this phases the content of Ni and Cr charge not monotonously from alloy to ceramic which shows strong chemical effects (the selective affinity of Cr and Ni). The concentration of Cr after the alloy surface increases in a 1-1.5 microns layer, where its concentration is higher than at the alloy, while the concentration of Ni decrease in this layer. Than at the ceramic side of the reaction zone the concentration of Ni increases in a 1-1.5 microns wide layer where its concentration is near upon that one in the alloy.

AB - In this investigation we observed the interface between Wiron 99 (Bego) dental Ni-Cr alloy and Vision (Wohlwend AG) ceramic opaquer with SEM. In the system there are intermediate phases coming from a solid phase rection which play an essential role in the metal-ceramic bond. The analytical methods showed that in this phases the content of Ni and Cr charge not monotonously from alloy to ceramic which shows strong chemical effects (the selective affinity of Cr and Ni). The concentration of Cr after the alloy surface increases in a 1-1.5 microns layer, where its concentration is higher than at the alloy, while the concentration of Ni decrease in this layer. Than at the ceramic side of the reaction zone the concentration of Ni increases in a 1-1.5 microns wide layer where its concentration is near upon that one in the alloy.

UR - http://www.scopus.com/inward/record.url?scp=0033110051&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0033110051&partnerID=8YFLogxK

M3 - Article

VL - 92

SP - 121

EP - 127

JO - Fogorvosi szemle

JF - Fogorvosi szemle

SN - 0015-5314

IS - 4

ER -