Abstract

The composition of the passive layer on aluminium and reformation of this layer during cathodic polarization were investigated by radiotracer and electrochemical methods in the presence of sulphate and chloride ions. Chloride ion is not ab- or adsorbed on the passive layer but, attacks this layer as a chemical reaction partner. Therefore, the pitting corrosion of aluminium and its alloys is a combined electrochemical and chemical process. The cathodic reformation of passive layer is indicated by the changing of the concentration of bonded chloride ion, the changing of hydrogen overvoltage as well as the shift of Eπ potential.

Original languageEnglish
Pages (from-to)855-859
Number of pages5
JournalElectrochimica Acta
Volume34
Issue number6
DOIs
Publication statusPublished - 1989

Fingerprint

Pitting
Aluminum
Chlorides
Aluminum alloys
Ions
Corrosion
Cathodic polarization
Sulfates
Protons
Chemical reactions
Hydrogen
Chemical analysis

ASJC Scopus subject areas

  • Chemical Engineering(all)
  • Analytical Chemistry
  • Electrochemistry

Cite this

Electrochemical study of the pitting corrosion of aluminium and its alloys-II. Study of the interaction of chloride ions with a passive film on aluminium and initiation of pitting corrosion. / Tomcsányi, L.; Varga, K.; Bartik, I.; Horányi, H.; Maleczki, E.

In: Electrochimica Acta, Vol. 34, No. 6, 1989, p. 855-859.

Research output: Contribution to journalArticle

@article{6b645f36a6c446db8f9d90e88b73116a,
title = "Electrochemical study of the pitting corrosion of aluminium and its alloys-II. Study of the interaction of chloride ions with a passive film on aluminium and initiation of pitting corrosion",
abstract = "The composition of the passive layer on aluminium and reformation of this layer during cathodic polarization were investigated by radiotracer and electrochemical methods in the presence of sulphate and chloride ions. Chloride ion is not ab- or adsorbed on the passive layer but, attacks this layer as a chemical reaction partner. Therefore, the pitting corrosion of aluminium and its alloys is a combined electrochemical and chemical process. The cathodic reformation of passive layer is indicated by the changing of the concentration of bonded chloride ion, the changing of hydrogen overvoltage as well as the shift of Eπ potential.",
author = "L. Tomcs{\'a}nyi and K. Varga and I. Bartik and H. Hor{\'a}nyi and E. Maleczki",
year = "1989",
doi = "10.1016/0013-4686(89)87119-1",
language = "English",
volume = "34",
pages = "855--859",
journal = "Electrochimica Acta",
issn = "0013-4686",
publisher = "Elsevier Limited",
number = "6",

}

TY - JOUR

T1 - Electrochemical study of the pitting corrosion of aluminium and its alloys-II. Study of the interaction of chloride ions with a passive film on aluminium and initiation of pitting corrosion

AU - Tomcsányi, L.

AU - Varga, K.

AU - Bartik, I.

AU - Horányi, H.

AU - Maleczki, E.

PY - 1989

Y1 - 1989

N2 - The composition of the passive layer on aluminium and reformation of this layer during cathodic polarization were investigated by radiotracer and electrochemical methods in the presence of sulphate and chloride ions. Chloride ion is not ab- or adsorbed on the passive layer but, attacks this layer as a chemical reaction partner. Therefore, the pitting corrosion of aluminium and its alloys is a combined electrochemical and chemical process. The cathodic reformation of passive layer is indicated by the changing of the concentration of bonded chloride ion, the changing of hydrogen overvoltage as well as the shift of Eπ potential.

AB - The composition of the passive layer on aluminium and reformation of this layer during cathodic polarization were investigated by radiotracer and electrochemical methods in the presence of sulphate and chloride ions. Chloride ion is not ab- or adsorbed on the passive layer but, attacks this layer as a chemical reaction partner. Therefore, the pitting corrosion of aluminium and its alloys is a combined electrochemical and chemical process. The cathodic reformation of passive layer is indicated by the changing of the concentration of bonded chloride ion, the changing of hydrogen overvoltage as well as the shift of Eπ potential.

UR - http://www.scopus.com/inward/record.url?scp=0024686256&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0024686256&partnerID=8YFLogxK

U2 - 10.1016/0013-4686(89)87119-1

DO - 10.1016/0013-4686(89)87119-1

M3 - Article

AN - SCOPUS:0024686256

VL - 34

SP - 855

EP - 859

JO - Electrochimica Acta

JF - Electrochimica Acta

SN - 0013-4686

IS - 6

ER -