A differential scanning calorimetry study of the release of stored energy in an AlFe alloy

J. Lendvai, G. Honyek, A. Juhász, I. Kovács

Research output: Contribution to journalArticle

5 Citations (Scopus)
Original languageEnglish
Pages (from-to)943-946
Number of pages4
JournalScripta Metallurgica
Volume19
Issue number8
DOIs
Publication statusPublished - 1985

Fingerprint

Calorimetry
Differential scanning calorimetry

ASJC Scopus subject areas

  • Engineering(all)

Cite this

A differential scanning calorimetry study of the release of stored energy in an AlFe alloy. / Lendvai, J.; Honyek, G.; Juhász, A.; Kovács, I.

In: Scripta Metallurgica, Vol. 19, No. 8, 1985, p. 943-946.

Research output: Contribution to journalArticle

@article{76eb10acd11647cb8f3803953a5cdf48,
title = "A differential scanning calorimetry study of the release of stored energy in an AlFe alloy",
author = "J. Lendvai and G. Honyek and A. Juh{\'a}sz and I. Kov{\'a}cs",
year = "1985",
doi = "10.1016/0036-9748(85)90288-1",
language = "English",
volume = "19",
pages = "943--946",
journal = "Scripta Materialia",
issn = "1359-6462",
publisher = "Elsevier Limited",
number = "8",

}

TY - JOUR

T1 - A differential scanning calorimetry study of the release of stored energy in an AlFe alloy

AU - Lendvai, J.

AU - Honyek, G.

AU - Juhász, A.

AU - Kovács, I.

PY - 1985

Y1 - 1985

UR - http://www.scopus.com/inward/record.url?scp=0022108102&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0022108102&partnerID=8YFLogxK

U2 - 10.1016/0036-9748(85)90288-1

DO - 10.1016/0036-9748(85)90288-1

M3 - Article

AN - SCOPUS:0022108102

VL - 19

SP - 943

EP - 946

JO - Scripta Materialia

JF - Scripta Materialia

SN - 1359-6462

IS - 8

ER -